Product Details:
|
| Material: | UNS S32750,S32900,S31803,S31500 | Standard: | A789/SA789, A790/SA790 |
|---|---|---|---|
| Type: | Seamless,Welded | OD: | 1/4inch~24inch |
| Wall Thickness: | SCH10S , SCH10, SCH20, SCH30, SCH40S... | Application: | Heat Exchangers And Coolers |
| Surface Treatment: | Varnish, Oil-dip, Passivation, Phosphating, Shot Blasting | Delivery Status: | Annealed, Normalized, Normalized+Tempered, Etc |
| Highlight: | stainless steel pipe,stainless steel round tube |
||
ASME SA789 UNS S31803 ASTM A790 S31803 Stainless Steel Tubing Duplex Stainless Steel Pipe / Tube 19.05 * 2.1mm
Product Standard: ASME SA789, ASTM A790
Main steel grades: UNS S31803
Application:
Chemical processing, Transport and Storage.
Oil and gas exploration and offshore rigs.
Oil and gas refining.
Marine environments.
Pollution control equipment.
Pulp and paper manufacturing
Chemical process Plant
Features:
1.Superior resistance to general and local corrosion, especially to stress corrosion, pitting corrosion, crevice corrosion, corrosion fatigue and abrasion & corrosion.
2.Good weldability
3.Good mechanical properties
4.Excellent intergranular corrosion resistance
5.High cost-effectiveness, long life time
Chemical Composition & Physical Properties:
| Grade |
C max |
Si max |
Mn max |
P max |
S max |
Cr | Ni | Mo | N |
| UNS S32750 | 0.030 | 0.8 | 1.2 | 0.030 | 0.015 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 |
| UNS S31803 | 0.030 | 1.0 | 2.0 | 0.020 | 0.020 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 |
| UNS S31500 | 0.030 | 1.0 | 1.2-2.0 | 0.030 | 0.030 | 18.0-19.0 | 4.5-5.5 | 2.5-3.5 | 0.05-0.10 |
| Grade | Y.S.MPa min | T.S.Mpa min | Elongation % | Hardness HRC |
| UNS S32750 | 550 | 800 | 15 | 20 |
| UNS S31803 | 450 | 620 | 25 | 20 |
| UNS S31500 | 440 | 630 | 30 | 20 |
Mark: As required.
Inspection and Test: chemical composition test, mechanical properties test(tensile, yield, elongation), process properties test(flatting, flaring, bending, hardness, impact, etc.), appearance and size test, non-destructive inspection test, hydrostastic test.
Delivery status: Annealed, normalized, normalized+Tempered, etc.
Surface treatment: oil impregnation, paint, passivation, phosphating, shot blasting etc.
Packing: Exporting package/wooden box /as requirement.
![]()
Contact Person: Mrs. Yana Dong
Tel: 13661003712, 86-10-5712 1108, 5718 5998